Double Poured Indefinite Chilled Rolls DPIC Rolls are designed with working layer of hard alloy iron and soft grey iron according to the needs. They are available with shell matrix with distribution of graphite and carbides imparts. These wear resistant rolls are available in stable shapes with excellent surface finishing. With excellent mechanical properties along with resistance to thermal & mechanical loads, these Double Poured Indefinite Chilled Rolls DPIC Rolls provide the best performance.
Technical details
HARDNESS | C% | MN% | SI% | CR% | NI% | MO% | S% |
---|---|---|---|---|---|---|---|
70-75 (DPIC) | 3.10-3.40 | 0.60-0.90 | 0.70-1.10 | 1.20-1.60 | 2.50-4.00 | 0.25-0.40 | 0.050 MAX |
75-80 (DPIC) | 3.10-3.40 | 0.60-0.90 | 0.70-1.10 | 1.40-1.80 | 2.50-4.50 | 0.25-0.40 | 0.050 MAX |
80-85 (DPIC) | 3.20-3.50 | 0.60-0.90 | 0.70-1.00 | 1.60-1.90 | 4.00-4.50 | 0.25-0.40 | 0.050 MAX |